Plasma Spray Coatings

Boeing Commercial Aircraft Group:

  • BMS 10-67, Type I

Pratt & Whitney Canada:

  • CPW 33-5 on Steel, Nickel and Cobalt Alloys
  • CPW 33-13 on Steel, Nickel, Cobalt and Titanium Alloys
  • CPW 33-16 on Steel, Nickel, Cobalt and Titanium Alloys
  • CPW 33-18 on Steel, Nickel and Cobalt Alloys
  • CPW 33-35 on Aluminum and Magnesium Alloys
  • CPW 33-37 on Steel, Nickel, Cobalt, Aluminum and Magnesium Alloys
  • CPW 33-48 on Steel, Nickel and Cobalt Alloys
  • CPW 33-48 on Ti and Ti Alloys
  • CPW 33-78 on Steel, Nickel and Cobalt Alloys
  • CPW 385 on Steel, Nickel and Cobalt Alloys
  • CPW 518 on Steel, Nickel, Cobalt Alloys and Titanium Alloys
  • CPW 524
  • CPW 535
  • CPW 672

Pratt & Whitney USA:

  • PWA 53-5 limited to Steel, nickel and cobalt base alloys.

Siemens Westinghouse

  • Spec 83263X3: MCrAlY – BN – Polyester Abaradable
  • Spec 83262A3: CoNiCrAlY
  • Spec 83342NU: Ceramically Bonded Al Coating with Chromate / Phosphate Top Coat
  • Spec 83260X1: 410 Stainless Steel
  • Spec 83262Y4: Stellite 6
  • Spec 83324Z1: CuNiIn
  • Spec 83269A4: Chromium Carbide

Rolls Royce (RR Energy Gas Turbine Sub Tier Supplier)

  • RPS300
  • RPS427
  • RPS629
  • RRU18

SAFRAN Group (Messier-Bugatti)

  • HVOF WC/Co/Cr 86-10-4
  • IFC 40-818-02

Bell Helicopter

  • BPS4463 (Tungsten Carbide Coatings)

Inorganic Paint Treatment:

Pratt & Whitney Canada:

CPW 420-12, -14, -22, -24, -52, -1A and -2A

Shot Peening:

Pratt & Whitney Canada:

  • AMS 2430 (Steel Shot)
  • AMS 2430 (Glass Beads)

ITP:

  • ITP - Application of Plasma Coating
  • ITP - Application of Thermal Spray Coatings with Plasma Technique
  • ITP Thermal Spray of Abradable Coatings

Share this post

Submit to DiggSubmit to FacebookSubmit to Google PlusSubmit to TwitterSubmit to LinkedIn
brands
Site design by:
MainlySunny.com
Site powered by: Joomla