Equipment list
Four (4) robotized acoustical thermal spray booth equipped with Fanuc robots
- Two (2) Sulzer plasma spray system 9MC
- Two (2) Sulzer HVOF spray system DJC
- Two (2) Miller plasma spray system
- One (1) Thermach plasma spray system
Sand Blasting
- Five (5) Blasting Cabinets – From 24’’x 24’’x 24’’ to 36’’x 36’’x 48’’
- Two (2) Walk-in chambers – 15’ x 15’ / 11’ x 14’
Peening
- Two (2) Cabinet for shot peening 36’’x 36’’x 48’’ / 24’’x 24’’x 24’’
- One (1) Walk-in chamber for glass bead peening – 11’ x 14’
Curing Oven
- Two (2) electrical oven. Max. temperature: 650o F . 7’x 7’ x 10’
- One (1) gas-fired oven. Max. temperature: 650o F . 7’x 7’ x 10’
Machine shop
- One (1) Cylindrical Grinder 12’’x 60’’
- One (1) Lathe 12’’x 48’’
- One (1) Supfina Super finisher
Laboratory
- Mount press
- Polishing machine
- Microscopes
- Hardness and micro-hardness testers
- Tensile test machine
- Cut off machine