VAC AERO’s Boucherville, Quebec facility has long held thermal spray and inorganic paint approvals for a variety of coating applications. Recently, the facility has become approved for a complementary grinding capability that allows it to act as a one-stop shop for applying and finishing chrome oxide coatings and paint used on turbine shafts and seal runners. […]