OAKVILLE, Ontario, (January 8, 2010) – VAC AERO’s Boucherville, Quebec, Canada-based Coatings division recently received two new approvals for coatings and chemical processing. The facility was qualified to the stringent SAE Aerospace Standard AS70003 for Coatings and for Chemical Processing. These two new approvals have now been added to the many other heat treating and coating accreditations that VAC AERO has acquired throughout the years. VAC AERO’s facilities in Quebec and Poland offer thermal spray coatings (plasma and HVOF), grinding and inorganic coating services to international Aerospace and other high-tech companies.