Model |
Width |
Height |
Length |
Standard Load Capacity @ 2400 ºF |
|
VAH 1212 |
8” (205mm) |
9” (230mm) |
12” (305mm) |
60 lbs (27 kgs) |
|
VAH 1220 |
8” (205mm) |
9” (230mm) |
20” (510mm) |
60 lbs (27 kgs) |
|
VAH 2024 |
16” (405mm) |
12” (305mm) |
24” (610mm) |
300 lbs (136 kgs) |
|
VAH 2224 |
18” (460mm) |
14” (355mm) |
24” (610mm) |
300 lbs (136 kgs) |
|
VAH 2636 |
23” (585mm) |
18” (460mm) |
36” (915mm) |
750 lbs (340 kgs) |
|
VAH 3436 |
24” (610mm) |
24” (610mm) |
36” (915mm) |
1,000 lbs (454 kgs) |
|
VAH 3448 |
24” (610mm) |
24” (610mm) |
48” (1220mm) |
1,500 lbs (680 kgs) |
|
VAH 4848 |
36” (915mm) |
30” (760mm) |
48” (1220mm) |
2,500 lbs (1,134 kgs) |
|
VAH 4860 |
36” (915mm) |
30” (760mm) |
60” (1525mm) |
3,000 lbs (1,361 kgs) |
|
VAH 4872 |
36” (915mm) |
30” (760mm) |
72” (1830mm) |
3,500 lbs (1,588 kgs) |
|
VAH 5050 |
36” (915mm) |
36” (915mm) |
50” (1270mm) |
3,000 lbs (1,361 kgs) |
|
VAH 5872 |
40” (1015mm) |
36” (915mm) |
72” (1830mm) |
3,500 lbs (1,588 kgs) |
|
VAH 6648 |
48” (1220mm) |
48” (1220mm) |
48” (1220mm) |
2,500 lbs (1,134 kgs) |
|
VAH 6660 |
48” (1220mm) |
48” (1220mm) |
60” (1525mm) |
4,000 lbs (1,814 kgs) |
|
VAH 6672 |
48” (1220mm) |
48” (1220mm) |
72” (1830mm) |
4,000 lbs (1,814 kgs) |
|
VAH 7672 |
54” (1370mm) |
54” (1370mm) |
72” (1830mm) |
4,000 lbs (1,814 kgs) |