OAKVILLE, Ontario, (January 8, 2010) – VAC AERO’s Boucherville, Quebec, Canada-based Coatings division recently received two new approvals for coatings and chemical processing. The facility was qualified to the stringent SAE Aerospace Standard AS70003 for Coatings and for Chemical Processing. These two new approvals have now been added to the many other heat treating and […]